Bi系2201相の機械的粉砕と再生成過程(II)
各種置換体の比較
新苗 稔展高田 潤池田 靖訓坂東 尚周
著者情報
ジャーナル フリー

1993 年 40 巻 11 号 p. 1065-1068

詳細
抄録

Mechanical grinding and the reformation from ground powder of the "2201" phase doped Pb, Ca and Ba were examined by XRD and DTA. The "2201" solid solutions changes easily into fine powder by mechanical grinding. The Ca-or Ba-substitution for Sr tends to suppress the formation of SrCO3 from the ground powder on mechanical grinding in air. The formation of Bi2CuO4 at 400°C and the reformation of the original "2201" phase at 800°C seem to be common for the "2201" solid solutions. The ground powder consists of not amorphous powder but ultra-fine crystals. Each crystal has a diameter of 30 to 100 Å and a thickness of one unit cell or a half unit cell length and thermally unstable.