粉体および粉末冶金
Online ISSN : 1880-9014
Print ISSN : 0532-8799
ISSN-L : 0532-8799
MIMにおけるAlSl 4600鋼の黒鉛添加による炭素量制御
天野 隆嗣村田 泰之杉山 大吾和出 昇木村 浩二
著者情報
ジャーナル オープンアクセス

1997 年 44 巻 5 号 p. 411-415

詳細
抄録
Debinding process as well as carbon in alloy powder has great effects on carbon content in final products using MIM process.
This paper describes the behavior of carbon and oxygen in debinding and sintering process by varing amount of graphite addition in AISI 4600 steel compounds.
The results are summarized as follows:
(1) Proper amount of carbon and oxygen in compounds makes possible to progress their removal by CO reaction in sintering process.
(2) Graphite addition to AISI 4600 steel compounds enables the control of carbon and oxygen content in fmal products under proper debinding conditions.
著者関連情報
© 社団法人粉体粉末冶金協会

本論文はCC BY-NC-NDライセンスによって許諾されています.ライセンスの内容を知りたい方は,https://creativecommons.org/licenses/by-nc-nd/4.0/deed.jaでご確認ください.