Nd-Fe-B系等方性HDDR磁石粉末の磁気特性に及ぼす出発合金組織の影響
森本 耕一郎五十嵐 和則新妻 永一郎中山 亮治
著者情報
ジャーナル フリー

2001 年 48 巻 8 号 p. 730-735

詳細
抄録

We investigated influences of original alloy microstructure on magnetic properties of the isotropic HDDR (hydrogenation-decomposition-desorption-recombination)-treated Nd126Fe79.0Co2.4B6.0 powder by comparing two types of starting materials, i.e., the strip cast (SC) alloy and the conventional book-mold cast (BMC) alloy. It was found that utilizing the SC alloy can achieve better I-H loop squareness, and consequently higher remanence in the final powder. The powder prepared from the SC alloy exhibits a more uniform grain structure of the recombined Nd2Fe14B phase, which is thought to be closely related to its good loop squareness. The effect of using the SC alloy is supposed to be attributed to the complete elimination of α-Fe particles before the HDDR treatment.