2000 年 12 巻 3 号 p. 371-373
To develop the high temperature shape memory bi-ceramics, the thermal expansion test was performed for Si-C-O glassy tyranno fiber which shows high resistant to heat and oxygen. The reversible shape change can be observed for Si-C-O glassy fiber sample under 1573K and below 25MPa.