The Proceedings of the Symposium on Environmental Engineering
Online ISSN : 2424-2969
2003.13
Conference information
Characteristics of Sintering Ash in Incinerator
Yoshiaki MATSUZAWAShunichiro UENOKenichi TAHARAJunya NISHINONobuhiko KUBOTAMasafumi MIMURASadahiro YAMADA
Author information
Keywords: sintering, ash, lead, chromium, XRD
CONFERENCE PROCEEDINGS FREE ACCESS

Pages 131-134

Details
Abstract
Annealed bottom ash from municipal waste incineration was characterized for metal leaching. Influence of temperature, oxygen concentration in the atmosphere and treatment time on leaching behavior was investigated. Concentration of lead and chromium (VI) increased as temperature and oxygen concentration in atmosphere rose. Prolongation of treatment time caused increase of lead leaching and degrease of chromium (VI). Sintering experiment of 4 particle-size groups classified by sieves revealed influence of particle size on lead and chromium leaching. The experiment also showed correlation among concentration of lead in leachate, pH of leachate and amount of Gehlenite in ash observed by XRD.
Content from these authors
© 2003 The Japan Society of Mechanical Engineers
Previous article Next article