J0310205 蒸気タービン鋳鋼経年材の脆化特性
荒川 大輔松村 栄郎西田 秀高緒方 隆志
著者情報
会議録・要旨集 フリー

詳細
抄録
For instrumentals used at high temperature for long term, such as steam turbine of thermal power plant, it is indispensable to grasp these deterioration states, since a material deterioration of softening, causes strength reduction and embrittlement leads to a falloff of tolerance crack length, etc., advances gradually, even when the creep or creep fatigue are not actualized, in order to prevent a destruction. Although it has been reported, at the hot section with the operating temperature higher than 500 ℃, tensile and creep strength fall together with softening, the knowledge which is needed for future operation management, whether deterioration state will advance with increasing speed or saturate etc., is not acquired. In this study, for the reheat stop valve scrap wood used for more than 300,000 hours, we carried out a hardness testing, charpy impact test, etc., and investigated the deterioration and embrittlement status.
著者関連情報
© 2015 一般社団法人 日本機械学会
前の記事 次の記事
feedback
Top