The composite materials mixed with coal ash and Kucha clay were fabricated by Spark Plasma Sintering (SPS). By changing the ingredient ratio of coal ash and clay, the mechanical properties were investigated in terms of specific gravity, micro vickers hardness and bending strength. The composite material including coal ash 95% and clay 5% (mass%) sintered at firing temperature 1473K ON SPS showed the highest strength 87.5MPa in the bending test.