OS2113 疲労き裂を有する溶接継手の延命化技術の開発
笛木 隆太郎安部 央矩高橋 宏治古池 仁暢
著者情報
会議録・要旨集 フリー

詳細
抄録
The maximum crack size rendered harmless on the weld toe of type 316 stainless steel welded joint by conducting Portable Pneumatic needle-Peening (PPP) was estimated focusing on stress intensity factor of crack tip. Stress intensity factor of external force and that of residual stress introduced by conducting PPP were calculated by FEM analysis. Then, it was found that the maximum crack size rendered harmless is 1.44 mm by comparing the stress intensity factor of semi-circular slit and the threshold stress intensity factor. The estimate value coincided with the result of bending fatigue test.