Mini-C(T)試験片を用いた原子炉圧力容器溶接金属脆化評価手法における試験片形状の影響
*石嵜 貴大, 小畠 亨司, DOVAN LAM, 廣川 文仁, 高本 真一, 門間 健介, 神長 貴幸
著者情報
会議録・要旨集 認証あり

詳細
抄録

Surveillance tests (Charpy impact tests) are employed to evaluate material degradation of Reactor Pressure Vessel (RPV) by neutron irradiation. To secure the sufficient number of surveillance specimens, embrittlement evaluation technique of RPV by master curve method using miniature compact tension specimen (Mini-C(T) specimen) have been developed. Due to the Mini-C(T) specimen for weld metal may be obtained from an unused Charpy impact specimen for weld metal, there are cases in which V-notch is included in Mini-C(T) specimen for weld metal. Therefore, the effect of the specimen shape to fracture toughness was evaluated.