The Proceedings of the Materials and processing conference
Online ISSN : 2424-287X
2000.8
Session ID : 411
Conference information
411 Rotary Joint Produced by Shave-joining Method
Takezo SASAKIKeisuke KANNOTerufumi MACHIDA
Author information
CONFERENCE PROCEEDINGS FREE ACCESS

Details
Abstract
Instead of costly conventional bonding methods a new manufacturing process was developed for high-performance rotary joint, which was an important element in machine system to pass through oil and other liquors. The mechanical seal of ceramics such as Al_2O_3,TiB_2,SiC and Zr_2O_3 was shave-joined with austenitic stainless steel housings for stator or rotor, comparing with a seal of cemented carbide alloy. The joining temperature of steel is at 100-600℃ and shaving depth is selected from the value of 0.15-0.5mm. The developed rotary joint was confirmed to possess sufficient properties required for the practical use: high joining strength and the stability.
Content from these authors
© 2000 The Japan Society of Mechanical Engineers
Previous article Next article
feedback
Top