凝結調整剤を用いたスラッジの有効利用に関する研究
中本 純次戸川 一夫三岩 敬孝
著者情報
ジャーナル フリー

2000 年 49 巻 10 号 p. 1121-1126

詳細
抄録

As for the effective utilization of sludge water containing cement and fine particles of aggregate, JIS A 5308 permits now the usage under 3 percent as solids for the unit content of cement. This study, in order to utilize the larger quantity of sludge water than that now allowed in the mixing plants, is to obtain the basical data on the properties of fresh concrete and of hardened concrete. Especially, in order to stabilize the quality of sludge by preventing hardening of sludge due to the hydration of cement particles, the effect of setting retarder has been discussed experimentally. From the results of this study, it was clarified that a good quality concrete could be obtained even though the sludge mass of 9% and the sludge age of 3 days, provided that setting retarder was used adequately.