青銅粉充てんポリアセタール/ポリエチレン(LDPE,HDPE,HMWHDPE)ブレンドの限界pv値と摩擦面挙動
高橋 博正斎藤 篤
著者情報
ジャーナル フリー

2003 年 52 巻 4 号 p. 419-426

詳細
抄録

To improve the pv limit of polymers, filled polyacetal (POM) and POM/polyethylene (PE) blends were studied. The fillers used were amino silane coupling agent treated and untreated bronze powder. And low density polyethylene (LDPE), high density polyethylene (HDPE) and high molecular weight high density polyethylene (HMWHDPE) were used as blended polymers in POM. Sliding tests were performed in a thrust washer type testing apparatus under unlubricated conditions. Frictional surfaces of a slider and specimens were investigated by XPS, EPMA and FT-IR. The additions of bronze powder and PE (LDPE, HDPE) in POM remarkably improved pv limit. The inclusion of bronze powder in POM/PE (LDPE, HDPE, HMWHDPE) blends and treating its bronze powder with amino silane coupling agent raised pv limit. And the pv limit of POM+25mass%HDPE+20mass%Br (treated) was approximately six times higher than that of POM. It was suggested that the POM film and the POM/PE mixed film produced in the frictional interface contributed to the elevation of pv limit.

著者関連情報
© 日本材料学会
前の記事 次の記事
feedback
Top