Abstract
In order to increase the penetration of TIG Arc Weld, laser activating process was devised. As the result of the welding with the devised process, deeper penetration weld, depth > 5 mm, aspect ratio > 0.7 under the condition of I=150A, v=2 mm/s for example, was obtained.