Abstract
Residual stress distributions at piping weld caused by repair welding were obtained from experiments and FE analyses. Repair welding at the outer surface caused increase of tensile stress at the inner surface. The change in residual stress was evaluated quantitatively by varying the groove depth and length of repair welding.