Preparation and Optical Properties of La3PO7:Eu3+ Nanophosphors Synthesized by Combustion Method
Ngo K. K. MinhTran B. LuanLam T. K. GiangNguyen T. ThanhTran T. K. ChiDariusz HreniakNgo Q. LuanNguyen Vu
著者情報
ジャーナル フリー HTML

2020 年 61 巻 8 号 p. 1564-1568

詳細
抄録

Eu3+ doped La3PO7 nanoparticles were successfully synthesized under facial combustion method. The nano-phosphors then were characterized by some techniques including X-ray diffraction (XRD), scanning and transmission electron microscopy (SEM and TEM), photoluminescence spectrum (PL), and lifetime decay. SEM and TEM micrographs reveal exhibit of the La3PO7: Eu3+ nanopowders in spherical morphology with an average size of about 20 nm, matching with Scherrer’s formula calculation. Otherwise, the influence of annealing temperature and concentration of Eu3+ ions on optical characteristics of Eu3+ was doped La3PO7, and optical properties were investigated too. The photoluminescence shows the strong red emission originating from the 5D07FJ (J = 1, 2, 3, and 4) transitions of Eu3+ and the 614 nm emission from the 5D07F2 electronic dipole transition is dominant.

Fullsize Image
著者関連情報
© 2020 The Japan Institute of Metals and Materials
前の記事 次の記事
feedback
Top