Abstract
Al2O3/ Ni nanocomposites were sintered by PECS (Pulse Electric Current Sintering) method in a vacuum of 4.5X10-5 Torr. We were carried out annealing 800°C, 1000°C, and 1200°C. Relative densities of all samples were larger than 95% of the theoretical density. The values of fracture strength were decreased with increase annealing temperature. However, the values of fracture toughness of annealed specimens at 800°C are higher than that of without annealing specimen.