Abstract
Gas-pressure sintering condition of silicon nitride with additives of 8%-lutetium oxide and 2%-silica was studied under 0.9 MPa of nitrogen pressure. Density of the sintered body was around 3. 4 g/cm3 when the sintered temperature was 2050°C.It was suggested that there is an optimum silica content for the powder bed.