亜鉛揮発回収法の基礎的研究 (続)
天沼 〓加藤 清二
著者情報
ジャーナル フリー

1958 年 74 巻 838 号 p. 253-256

詳細
抄録

We studied the reducibilities of zinc compounds, such as ZnAl2O4and ZnS and of copper slag at Naoshima Smelter underCOatmosphere. These samples and carbon powder were mixed with or without CaCO3. ZnAl2O4was stable and reduced only 30% at 1050°C. ZnS was reduced 90% when mixed with CaCO3, but only 20% without CaCO3, but. only 20% without CaCO3 at 900°C. The reducibility of zinc in Cu-slag was nearly as same that of Pb-slag and ZnFeSiO4. We also studied the decomposition of Zn-ferrite when heated with CaCO3and the prevention of formation of Zn-ferrite from mixture of ZnO, Fe2O3and CaCO3. In both cases, free ZnO was leached 60-70% from the samples heated at 1100°C.