鉄と鋼
Online ISSN : 1883-2954
Print ISSN : 0021-1575
ISSN-L : 0021-1575
技術報告
高Ni合金連続鋳造スラブ切断装置の改善
宮崎 芳春水野 建次本郷 敦哉石井 照彰轟 秀和
著者情報
ジャーナル オープンアクセス

2007 年 93 巻 7 号 p. 518-523

詳細
抄録
An improvement has been carried out to minimize the time for cutting continuously cast slabs in high-Ni alloy by means of a torch-cut equipped with Fe and Al powder supply. Two major reasons why it was so tough to cut the slabs in high-Ni alloy were considered. Firstly, heat generation by torch-cut is insufficient to keep burning a slab for high-Ni alloy because Ni is a metal nobler than Fe or Cr. Secondly, fluidity of the flown melt formed by torch-cut of slab is lower for high-Ni alloy than for low-Ni stainless steel. The formed flown melt consists of a mixture of molten alloy and oxides. The flown melt for high-Ni alloy includes higher ratio of solid oxides which lowers the fluidity. In order to cut the slab against low fluidity of the flown melt, the cutting device was improved by increasing ability to supply combustion gas and powder. In addition, the powder ratio of Al to Fe was optimized as 25 mass%. Consequently, the improvement succeeded in shortening the time for cutting a slab to half for high-Ni alloy.
著者関連情報
© 2007 一般社団法人 日本鉄鋼協会

This article is licensed under a Creative Commons [Attribution-NonCommercial-NoDerivatives 4.0 International] license.
https://creativecommons.org/licenses/by-nc-nd/4.0/
前の記事 次の記事
feedback
Top