1957 年 43 巻 2 号 p. 142-145
To investigate the influence of Mo and V additions on the properties of Si-Cr-W shockresisting steel containing 0.55% carbon, 1.4% chromium and 2.1% tungsten, the authors measured the transformation point, quenching and tempering hardness, hardenability, rate of deformation, mechanical properties at elevated temperature and microstructures.
From the results of these experiments, the authors ascertained that through the Mo and V additions to the Si-Cr-W shock-resisting steel, its properties were improved remarkably.