The precursor of calcium cobalt oxide thermoelectric material was fabricated by reflux method. Cobalt acetate and calcium acetate were used as starting materials. We investigated the calcination temperature to obtain Ca
3Co
4O
9 and the effect of temperature raising rate on size of grains.
抄録全体を表示