Characteristics of Fine Oxide Particles Produced by Ti/M (M=Mg and Zr) Complex Deoxidation in Fe–10mass%Ni Alloy
Andrey V. KarasevHideaki Suito
著者情報
ジャーナル フリー

2008 年 48 巻 11 号 p. 1507-1516

詳細
抄録

Characteristics of oxide particles produced by Ti/M (M=Mg and Zr) complex deoxidation have been studied in an Fe–10mass%Ni alloy as a function of holding time at 1600°C, followed by quenching. The size distributions for the particles having different compositions are compared with the particle size distribution in single deoxidation with Ti, Mg or Zr. In most experiments the composition of particles precipitated during rapid quenching was found to be non-equilibrium phase. The formation mechanism of primary and secondary deoxidation particles and the difference in the compositions of non-clustered and clustered particles are discussed. The effects of Ti addition, method of deoxidation and holding time at 1600°C on particle size distributions in Ti/M complex deoxidation experiments are studied.

著者関連情報
© 2008 by The Iron and Steel Institute of Japan
前の記事 次の記事
feedback
Top