Journal of Oral Tissue Engineering
Online ISSN : 1880-0823
Print ISSN : 1348-9623
ISSN-L : 1348-9623
ORIGINAL ARTICLES
Effect of Hydroxyapatite Fiber Material with Autogenous Bone Graft on Vertical Bone Augmentation
Junichi KIMURA, Makoto SHIOTA, Kazuhiro KON, Masaki FUJI, Hitoshi SATO, Shouhei KASUGAI
著者情報
ジャーナル フリー

2012 年 9 巻 3 号 p. 136-146

詳細
抄録
Purpose: The aim of this study was to examine effects of hydroxyapatite fiber (HF) combining with autogenous Bone on vertical bone augmentation.Materials and methods: Polytetrafluoroethylene chambers were fixed to the parietal bone on the right and left sides in thirty-six Japanese male white rabbits. HF only (30 or 60 mg) and combination of HF with autogenous bone from tibia at different ratios (30 mg bone/HF ratio: 3/1, 3/2, 1/1) were grafted into each chamber. Chambers were left empty in the negative control animals (empty group). Rabbits were sacrificed at 4 and 8 weeks. Then, total bone volume (TBV) of highly calcified bone region in the chamber was quantified with micro-CT analysis. Histomorphometric analysis was performed to evaluate the area of newly formed bone (BA). Statistical analysis was performed with the Student t-test and Tukey- Kramer's method.Results: In histology, newly formed bone conducted by HF showed a particular structure, and active bone regeneration was observed in the groups containing more HF at 8 weeks. From 4 weeks to 8 weeks BA was significantly reduced in the control, HF 30 mg and ratio 3/1 groups. At 8 weeks BA of HF 60mg was significantly higher than the one of HF30mg group.Conclusions: Combination of HF with autogenous bone was effective in vertical bone augmentation although optimal ratio of the combination needs further study.
著者関連情報
© 2012 by Japanese Association of Regenerative Dentistry
前の記事 次の記事
feedback
Top