1992 年 100 巻 1160 号 p. 581-584
(1) Izod impact test was proposed to evaluate the fracture energy of mode I failure of fiber-reinforced ceramics.
(2) By selecting the notch geometry of a specimen and the loading condition, the fracture of carbon fiber-reinforced silicon nitride resulted from mode I crack.