材料と環境
Online ISSN : 1881-9664
Print ISSN : 0917-0480
ISSN-L : 0917-0480
SUS 304鋼の高濃度塩化物水溶液応力腐食割れ中の高速脆性破壊
田村 宙治竹本 幹男
著者情報
ジャーナル フリー

1997 年 46 巻 4 号 p. 256-262

詳細
抄録
This research aims to study the SCC fracture dynamics of a AISI 304 steel in 42wt% MgCl2 solution at temperature at 413±4K using the advanced acoustic emission (AE) signal processing. AE signals (out-plane displacement) from the Mode-I fracture were monitored by the special AE monitoring system. Source wave was estimated by using the transfer function experimentally determined. It was revealed that the brittle fracture in size of 10 to 40μm generated at the maximum velocity of 40m/s.
著者関連情報
© 社団法人腐食防食協会
前の記事
feedback
Top