Al-8%Si 合金薄肉鋳物の500℃溶体化処理における析出Si 相の粒状化
森中 真行大城 直人宮尻 聡團野 瑛章
著者情報
ジャーナル フリー

2019 年 91 巻 8 号 p. 542-546

詳細
抄録

  Hypo-eutectic Al-Si alloy die casting is gradually being applied to manufacture automobile bodies and frames. However, since the cast product is thin, it is difficult to deal with distortion during heat treatment. Short-time heat treatment is a potential method for avoiding this. In order to develop a short-time heat treatment technique to granulate the eutectic Si phase without coarse precipitate phase, we investigated the number of coarse precipitate phases and behavior of morphological change in this study. As a result, it was clarified that the number coarse precipitate phases decreases with time while the plate shape is gradually changed to granular shape, after the number of coarse precipitate phases sharply increased at the beginning of heat treatment. As the preferred heat treatment condition, we proposed retention of 60 minutes at about 500℃.

著者関連情報
© 2019 公益社団法人 日本鋳造工学会
前の記事 次の記事
feedback
Top