No.14 ハイパーコール製造プロセスにおける急速昇温抽出の効果(熱分解・コークス(4))
堺 康爾木下 繁吉田 拓也奥山 憲幸濱口 眞基菊池 直樹
著者情報
会議録・要旨集 フリー

詳細
抄録
Hyper-coal (HPC) is an ash-free coal produced by the solvent de-ashing technology. Coal is thermally (360-420℃) extracted into the coal-derived solvent (two ring aromatics). HPC has excellent thermoplasticity and large potential for coke additive to make a strong coke. The yield of HPC depends on the coal solubility. And the solvent must be recovered completely by distillation. Therefore, it is important for HPC process to use a solvent that have not only high solubility of coal but also enough recovery ratio. In this study, we focused on the extraction heating rate condition. In conventional method, after coal and solvent are mixed, the slurry is heated. In this method, the heating rate is lower than 100 K/min. In order to increase the heating rate solvent is heated to higher temperature than the extraction temperature beforehand, and coal is thrown into high temperature solvent. The latter method enables to increase the heating rate at > 100 K/min., and the consequent coal extraction yield increased with increasing the heating rate.
著者関連情報
© 2014 一般社団法人 日本エネルギー学会
前の記事 次の記事
feedback
Top