主催: 日本エネルギー学会 石炭科学部会, 日本エネルギー学会 コークス工学研究部会
共催: 日本学術振興会 石炭・炭素資源利用技術第148委員会, 化学工学会 エネルギー部会, 日本エネルギー学会 重質油部会
後援: 東北大学
会議名: 第51回石炭科学会議
回次: 51
開催地: 東北大学工学部 青葉記念会館
開催日: 2014/10/22 - 2014/10/23
In a series of studies into the development of an efficient and selective recovery process for gold that eliminates the need for water, the release behavior of gold from an incinerated sewage sludge ash heated to between 100 and 1000℃ under a chlorine gas stream was investigated. A release of gold was observed above 600℃, with all gold being transferred to the gas phase at 1000℃. The addition of solid carbon to the incinerated ash reduced this initial release temperature to 400℃, with all gold being released into both the gas phase and solid carbon at 700℃. Subsequent optimization of the reaction conditions to maximize the amount of gold reporting to the solid carbon determined that the mixture of incinerated ash and carbon should first be heated to a terminal temperature of 800℃ under a nitrogen gas stream. Upon reaching this temperature, the gas stream should be switched from chlorine to nitrogen, and the mixture held at 800℃ for 1 h. Scanning electron microscopy and X-ray diffraction measurements confirm that this produces a distribution of fine metallic gold over the carbon surface.