Abstract
The author herein discusses the corrosion rate of Cu-Zn system calculated from the heat of activation in the hydrogen electrode reaction and normal electrode potential and shows that it fairly consists with the experimental results and that the anomaly of hydrogen overvoltage in ε-phase is due to the structure of ε-phase itself.