Effects of alumina air-abrasion and acidic priming agents on bonding between SUS XM27 steel and auto-polymerizing acrylic resin
Yumi IshikawaNorihisa OhashiHiroyasu KoizumiNaomi TanoueNorihiro NishiyamaHideo Matsumura
Author information
Keywords: bonding, magnet, phosphate, steel
JOURNAL FREE ACCESS

2007 Volume 49 Issue 3 Pages 191-195

Details
Abstract
The purpose of this study was to evaluate the effects of functional monomers contained in the primers, as well as alumina particle abrasion on bonding between stainless steel and acrylic resin. SUS XM27 steel was primed with one of the following materials; Alloy Primer, Estenia Opaque Primer, M. L. Primer, and Super-Bond Liquid. Steel disks were either ground flat or alumina-blasted, primed with one of the four agents, and bonded with an acrylic resin (Unifast Trad). Bond strength was determined both before and after thermocycling (2,000 or 20,000 cycles). Among the four priming agents, the Alloy Primer and Estenia Opaque Primer, both of which contain 10-methacryloyloxydecyl dihydrogen phosphate (MDP), exhibited better bonding performance than the others. Alumina air-borne particle abrasion considerably improved the durability of bonding between the steel and the resin material. It can be concluded that alumina blasting followed by priming with an MDP agent is recommended for bonding the resin and SUS XM27 steel. (J. Oral Sci. 49, 191-195, 2007)
Content from these authors
© 2007 by Nihon University School of Dentistry
Previous article Next article
feedback
Top