Abstract
To examine whether the surface reaction layer of titanium castings can be reduced by lowering the mold temperature during casting, we cast titanium at three mold temperatures, including an ultra-low temperature produced by cooling the mold with liquid nitrogen, then measured the tensile strength and elongation of the castings. The titanium was cast using a centrifugal casting machine, and the molds were incinerated according to the manufacturers' instructions. Castings were then made with the molds at 200°C, 600°C, and an ultra-low temperature (-196°C). The castability of titanium cast in the mold at the ultra-low temperature was good. The Vickers hardness near the surface layer of castings decreased as the mold temperature decreased. (J. Oral Sci. 43, 27-33, 2001)