2018 Volume 61 Issue 4 Pages 205-212
Vapor-phase dehydrogenation of ethanol to acetaldehyde was studied using Cu/SiO2 and ZnO/SiO2 catalysts prepared by the conventional impregnation method. Catalysts were characterized by XRD, nitrogen adsorption-desorption analysis, XPS, N2O-pulse method, CO2-TPD and C2H5OH-TPD. Use of copper ammonium complex for the preparation of Cu/SiO2 catalysts formed Cu particles on SiO2 too small for detection by XRD. The prepared Cu/SiO2 catalyst had high and selective dehydrogenation activity of ethanol to acetaldehyde. However, Cu/SiO2 catalyst was less stable at 350 °C due to sintering of Cu. Interestingly, a metal oxide catalyst, ZnO/SiO2, had fairly high and fully selective activity for dehydrogenation of ethanol to acetaldehyde. Furthermore, no changes in the activity and selectivity were observed for at least 6 h at 350 °C. The reaction pathways on the metal catalyst, Cu/SiO2, and the oxide catalyst, ZnO/SiO2, were studied by C2H5OH-TPD. Evolution of H2 was observed from ethanol contacted with Cu/SiO2 catalyst at 50 °C, suggesting dehydrogenation at this temperature. Desorption of acetaldehyde was observed above 200 °C. On the other hand, simultaneous desorption of H2 and acetaldehyde occurred on ZnO/SiO2 catalyst above 240 °C, suggesting that the rate determining step is the dissociative adsorption of ethanol at this temperature. Thus, the reaction pathways were very different for the metal catalyst and the oxide catalyst.