機械材料・材料加工技術講演会講演論文集
Online ISSN : 2424-287X
セッションID: 608
会議情報
608 アクリル系接着剤を用いた異種材料接合体の接着強度評価(OS 接着・界面)
平田 恭一木原 幸一郎杉林 俊雄田口 広一
著者情報
会議録・要旨集 フリー

詳細
抄録
The volume shrinkage ratio and the residual stress that occurs at the curing shrinkage of acrylic resin were measured. The volume shrinkage ratio was measured with the laser displacement detector system and the dilatometer. The volume shrinkage ratio of acrylic resin was about 16%. Most of the volume shrinkage resulted in about 12 minutes after the mixture. The residual stress in interface of adhesive layer was calculated by measuring the residual strain of adherend. The influence of the residual stress on the adhesive strength must be considered.
著者関連情報
© 2000 一般社団法人 日本機械学会