日本機械学会論文集 A編
Online ISSN : 1884-8338
Print ISSN : 0387-5008
不織布挿入型ハイブリッド複合材料の層間破壊じん性について : 第1報, モードI層間破壊じん性
李 丞桓金 永培野口 博司
著者情報
ジャーナル フリー

2001 年 67 巻 661 号 p. 1471-1476

詳細
抄録

Interlaminar fracture behavior of hybrid composites with non-woven carbon tissue is investigated under a Mode I loading condition with a DCB specimen. Hybrid composites are made by inserting non-woven tissue between prepreg layers. Two kinds of specimens are prepared from [0]24 and [012/ 012]. Here the symbol "/" means that non-woven carbon tissue is located at a 0/0 mid-plane of the specimen. An initial interlaminar crack is introduced to a mid-plane of the specimen. Interlaminar fracture toughness (GIC) of hybrid composites is compared with that of CFRP. GIC of hybrid composites is almost dependent on only that of matrix resin. The fracture surfaces of the specimens are observed with an optical microscope and SEM, and the failure mechanism is discussed.

著者関連情報
© 社団法人日本機械学会
前の記事 次の記事
feedback
Top