PREPARATION OF SILOXANE-CONTAINING VATERITE ⁄ POLY (LACTIC ACID) HYBRID BEADS BY ELECTROSPRAYING AND HA-COATING ON THEIR SURFACES
Jin NAKAMURAAkiko OBATAToshihiro KASUGA
著者情報
ジャーナル フリー

2010 年 24 巻 p. 1-5

詳細
抄録

Bead–shaped siloxane–containing vaterite (SiV) ⁄ poly (L–lactic acid) (PLLA) hybrid beads with ca. 40 – 130 μm in diameter were prepared by an electrospraying method. The beads included pores of ∼1 μm in diameter. SiV particles were embedded in the PLLA matrix. The beads containing 20 wt% of SiV showed the releasabilities of Si4+ and Ca2+ ions in a dilute acetic acid solution of pH 4. To improve cytocompatibility, the beads were coated successfully with a hydroxyapatite layer by soaking in simulated body fluid (SBF).