2003 Volume 54 Issue 10 Pages 689-692
Diamond synthesis onto iron substrate was tried by hot-filament chemical vapor deposition (HFCVD). Diamond can be synthesized at an atmospheric pressure by spraying a source gas onto an iron substrate with a nozzle. Diamond crystal grows to a size of about 20μm in 180 min. Diamond synthesized by the present method contains only a small amount of non-diamond carbon. Diamond synthesis on a silicon wafer is also enhanced by spraying a source gas onto a substrate like an iron case.