2008 年 59 巻 4 号 p. 265
Si was sublimated at 1400 degrees in a vacuum, and caused to react with the VGCF. Based on the mixed rate of Si, it became clear that sublimated Si reacts to the VGCF surface partially or fully, and forms the reaction phase of SiC. As a result of evaluating wettability, it became clear that SiC phase causes the molten magnesium alloy to have good wettability.