取鍋用真空吸引式除滓設備の操業
宮脇 芳治半明 正之白谷 勇介松田 安弘小松 喜美
著者情報
ジャーナル オープンアクセス

1984 年 70 巻 14 号 p. 1697-1703

詳細
抄録
BOF slag run into casting ladle at tapping gives disadvantageous effects in the succeeding steelmaking process, such as rephosphorization, low yield of alloy, and steel contamination in the form of inclusion at the stage of casting. Conventionally at NKK Fukuyama Works, dragger was applied to eliminate the slag mechanically. This mechanical method, however, had caused imperfect slag skimming, mechanical damage to casting ladle, steel loss, and temperature drop and so on.
To solve these problems, introduction of vacuum slag cleaner (VSC) for casting ladle was made. In September, 1982, NKK started the operation of VSC. And the monthly production through VSC was increased up to 50 000 tons of steel. Various effects of VSC treatment, such as reduction of aluminum consumption, less rephosphorization and better cleanliness of the steel, are discussed quantitatively in this study.
著者関連情報
© 一般社団法人 日本鉄鋼協会

This article is licensed under a Creative Commons [Attribution-NonCommercial-NoDerivatives 4.0 International] license.
https://creativecommons.org/licenses/by-nc-nd/4.0/
前の記事 次の記事
feedback
Top