The operation of prereduction fluidized bed combined with an in-bath smelting furnace was performed in NKK Fukuyama Works. Iron ore fines, such as sinter feed are directly charged into the fluidized bed. This fluidized bed was so designed as to form a dense bubbling bed and equip the circulating device. The reduction characteristics of iron ore fines were clarified through the operation in the integrated test plant. According to the above results and the simulation model based on the elutriation behavior, the appropriate residence time of coarse became 30-60 min to reduce the iron ore to 20-25% reduction degree in 800°C bed temperature. The effect of circulation of fines was not quantitatively clear in the test, but the favorable circulation ratio was estimated with a mathematical model. Moreover, it was found that the collection efficiency of cyclone was closely related to the yields of prereduced ore and the circulation ratio influenced on the losses of products.

Content from these authors
© The Iron and Steel Institute of Japan
Previous article Next article
feedback
Top