2015 Volume 34 Issue 5 Pages 611-617
In this study, we investigated the influence of light intensity on the surface-free energy and dentin bond strength of single-step selfetch adhesives. The adhesives were applied to the dentin surfaces of bovine mandibular incisors and cured with light intensities of 0 (no irradiation), 200, 400, and 600 mW/cm2. Surface-free energies were determined by measuring the contact angles of three test liquids placed on the cured adhesives. Dentin bond strengths of the specimens were also measured. Polymerization with a higher light intensity resulted in a lower surface-free energy of the cured adhesives. The greatest bond strength was achieved when a light intensity of 400 mW/cm2 or greater was used. Our data suggest that the surface-free energy and dentin bond strength of single-step self-etch adhesives are affected by light intensity of the curing unit.