CdTe films were prepared by simultaneous evaporation of Cd and Te using one boat. Films were deposited on glass substrates heated between 200 and 500 C. Film thickness, transmission, dark-and photocurrent were measured. X-ray diffraction techniques were used to analyze the structure and orientation of the films. These properties were related to the temperature of substrates and phosphorus added during evaporation.