Abstract
Thermo-sensitive copolymer consists of poly(2-ethoxyethyl vinyl ether) and poly(hydroxyethyl vinyl ether) (EOVE200–HOVE400), whose sol–gel transition temperature was 20.5 °C, was synthesized and its applicability to a drug delivery system was examined. Vitamin E (VE) was enclosed in EOVE200–HOVE400 and the release of VE was measured by varying the temperature 10⇔30 °C. There was no release of VE from EOVE200–HOVE400 at 30 °C, while VE was released when the temperature was reduced to 10 °C.