Comparison of Carbonate Apatite and β-tricalcium Phosphate (Resorbable Calcium Phosphates) Implanted Subcutaneously into the Back of Rats
Motohiko NAGAYAMAHiroshi TAKEUCHIYutaka DOI
著者情報
ジャーナル フリー

2006 年 25 巻 2 号 p. 219-225

詳細
抄録
Bioresorption and biocompatibility of carbonate apatites, both sintered and non-sintered (S-CAP and N-CAP) , and of sintered β-tricalcium phosphate (β-TCP) were compared by implanting particles of these materials into the back of adult rats. Bioresorption — when evaluated non-destructively with non-decalcified tissues using microfocus X-ray tomography — was essentially the same for N-CAP and β-TCP, while S-CAP exhibited statistically lower bioresorption at 2, 4, and 12 weeks postoperatively. Biocompatibility — when evaluated by ED1 immunostaining — was in the order of β-TCP > N-CAP > S-CAP. The intensity of ED1 immunostaining decreased with time, but persisted longer in β-TCP than in S-CAP and N-CAP, indicating that β-TCP produced the strongest and most enduring stimulation of macrophages. Although no statistical differences were found in tartrate-resistant acid phosphatase (TRAP) staining among the materials at each implantation period, the degree of TRAP staining for S-CAP was statistically greater at 12 weeks than at 2 and 4 weeks, indicating that osteoclast-like cells were in part responsible for the resorption of the carbonate apatite.
著者関連情報
© 2006 The Japanese Society for Dental Materials and Devices
前の記事 次の記事
feedback
Top