Effect of an internal coating technique on tensile bond strengths of resin cements to zirconia ceramics
Shuzo KITAYAMAToru NIKAIDORena MARUOKALei ZHUMasaomi IKEDAAkihiko WATANABERichard M. FOXTONHiroyuki MIURAJunji TAGAMI
著者情報
ジャーナル フリー

2009 年 28 巻 4 号 p. 446-453

詳細
抄録
This study was conducted to enhance the tensile bond strengths of resin cements to zirconia ceramics. Fifty-six zirconia ceramic specimens (Cercon Base) and twenty-eight silica-based ceramic specimens (GN-1, GN-1 Ceramic Block) were air-abraded using alumina. Thereafter, the zirconia ceramic specimens were divided into two subgroups of 28 each according to the surface pretreatment; no pretreatment (Zr); and the internal coating technique (INT). For INT, the surface of zirconia was coated by fusing silica-based ceramics (Cercon Ceram Kiss). Ceramic surfaces were conditioned with/without a silane coupling agent followed by bonding with one of two resin cements; Panavia F 2.0 (PF) and Superbond C&B (SB). After 24 hours storage in water, the tensile bond strengths were tested (n=7). For both PF and SB, silanization significantly improved the bond strength to GN-1 and INT (p<0.05). The INT coating followed by silanizaton demonstrated enhancement of bonding to zirconia ceramics.
著者関連情報
© 2009 The Japanese Society for Dental Materials and Devices
前の記事 次の記事
feedback
Top