The influence of zirconia coping designs on the fracture load of all-ceramic molar crowns
Yuji KOKUBOMitsuyoshi TSUMITATakamitsu KANOShunji FUKUSHIMA
Author information
JOURNAL FREE ACCESS

2011 Volume 30 Issue 3 Pages 281-285

Details
Abstract
This study investigated the influence of zirconia coping designs on the fracture load of all-ceramic crown. Four kinds of zirconia copings were designed (a: Conventional zirconia coping with flat occlusal surface: thickness of the each coping is 0.6 mm evenly, and at the cervical margin area, the coping is adjusted sharply so as to fit preparation margin, b: Conventional zirconia coping with shoulder collar of 1 mm: thickness of the each coping is 0.6 mm evenly, and there is a collar of 0.6 mm from the margin, c: Zirconia coping with following original cuspal configuration (concave): two inclined cusp planes, and at the cervical margin area, the coping is adjusted sharply so as to fit preparation margin, and d: Zirconia coping with supporting configuration on the occlusal area: supporting configuration against the occlusal force, and at the cervical margin area, the coping is adjusted sharply so as to fit preparation margin) and porcelain was fired. Vertical and lateral load were conducted until fracture. Coping design affected the fracture load; conventional uniform thickness coping design showed the lowest load (a), whereas cuspal configuration to perform even thickness of porcelain showed the highest fracture load both load directions (c).
Content from these authors
© 2011 The Japanese Society for Dental Materials and Devices
Previous article Next article
feedback
Top