Dental Materials Journal
Online ISSN : 1881-1361
Print ISSN : 0287-4547
ISSN-L : 0287-4547
Original Papers
In vitro wear resistance, hardness and elastic modulus of artificial denture teet
Pii SUWANNAROOPPisaisit CHAIJAREENONTNatthavoot KOOTTATHAPEHidekazu TAKAHASHIMansuang ARKSORNNUKIT
著者情報
ジャーナル フリー

2011 年 30 巻 4 号 p. 461-468

詳細
抄録
In this study, the wear resistance, hardness, elastic modulus, and the correlations between them of artificial denture teeth at the sub-enamel layer were examined. Four types of tested artificial denture teeth consisted of 3 conventional acrylic resin teeth (Cosmo HXL, Major Dent, and Yamahachi FX), 1 high cross-linked acrylic resin teeth (Trubyte Bioform IPN), 2 composite resin teeth (SR Orthosit PE, and Yamahachi PX), and 1 porcelain teeth (ACE Teeth). The two-body wear test was performed using a custom made pin on disc apparatus. Volume and weight loss were measured. Hardness and elastic modulus were also assessed by using a nanoindentation system. The results suggested wear resistance varied among the denture tooth materials. Wear resistance of high cross-linked acrylic resin teeth was the lowest. A definite relation between wear resistance and mechanical properties of materials could not be found in this study.
著者関連情報
© 2011 The Japanese Society for Dental Materials and Devices
前の記事 次の記事