Abstract
This study evaluated the shear bond strength (SBS) of a traditional orthodontic bracket bonding agent (Transbond XT) against two self-etch, self-adhesive systems (Maxcem Elite and Vertise Flow). Sixty premolar teeth and sixty brackets were randomly and equally divided into five groups: Transbond XT (TXT) as the control, Maxcem Elite (ME) without etching, ME with etching (ME/ Etch), Vertise Flow (VF) without etching, and VF with etching (VF/Etch). Respective SBS results of the five groups were 9.86±3.20, 4.67±2.94, 7.82±2.56, 2.55±0.77, and 7.89±1.17 MPa. SBS values of the new self-etch adhesive systems were significantly lower than the traditional etch-and-rinse control (p<0.005). However, no significant differences were found between TXT and the self-adhesives applied with etching (p>0.005). After debonding, ARI scores “0" and “1" were predominant in non-etched ME and VF groups. It was concluded that new self-etch, self-adhesive bonding systems require additional phosphoric acid application to achieve comparable SBS values as the traditional orthodontic bonding agent.
Content from these authors
© 2012 The Japanese Society for Dental Materials and Devices
Previous article Next article
feedback
Top