セラミックス二次元切削時のき裂進展長さおよびき裂進展抑止上限切込み深さ
円管の押広げ解を援用した場合の推定
水谷 勝己田中 芳雄
著者情報
ジャーナル フリー

1987 年 53 巻 11 号 p. 1758-1764

詳細
抄録
A crack extension problem based on the fracture mechanics is solved to estimate the length of downward extension of a crack and the upper limit of depth of cut preventing its extension in orthogonal cutting of ceramics. To solve the problem evidently in conjection with mechanical properties of the work, the stress field of the expansion of a cylindrical tube is successfully applied to the elasto-plastic tensile stress field in the work by the tool progress. It is shown that the length of the crack extension is uniquely determined by the combination among the depth of cut, the fracture toughness and the yield strength. The upper limit of depth of cut is found to be proportional with square of the ratio of the fracture toughness for micro crack-to-the yield strength. The estimated value of the upper limit of depth of cut coincides approximately with that of experiment for alumina ceramics and soda-lime glass.
著者関連情報
© 社団法人 精密工学会
前の記事 次の記事
feedback
Top