Dealloying of Cu-Zr-Ti Bulk Metallic Glass in Hydrofluoric Acid Solution
Hiroya AbeKazuyoshi SatoHiroshi NishikawaTadashi TakemotoMikio FukuharaAkihisa Inoue
Author information
JOURNAL FREE ACCESS

2009 Volume 50 Issue 6 Pages 1255-1258

Details
Abstract

The dealloying behavior of Cu60Zr30Ti10 metallic glass was investigated under free corrosion conditions using hydrofluoric acid (HF) solutions at room temperature. After immersing in HF solutions with various concentrations (0.05, 0.1, 0.5 and 1 M) for 300 s, color of all samples changed to be pinkish or peachy, which was ascribed to Cu based on the XRD patterns. According to the SEM-EDS study, HF immersion selectively leached the Zr and Ti elements, leaving Cu behind. Increasing the HF concentration increased the dealloying rate. Moreover, the HF concentration strongly influenced the surface morphology of the resulting Cu.

Content from these authors
© 2009 The Japan Institute of Metals and Materials