Name : [in Japanese]
Location : [in Japanese]
Date : December 09, 2016 - December 10, 2016
Pages 43-46
Ag and SnS were sequentially vapor-deposited on a glass substrate by a vacuum deposition method and heat-treated at 350 to 500℃ for 1 hour in an H2S atmosphere. From the XRD pattern, diffraction peaks of SnS crystal for precursor film, Ag2S crystal for the thin films annealed at 350 to 400℃, and Ag8SnS6 crystal for the thin films annealed at 400 to 500℃ could be confirmed.